Ubicación: Global + English
Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Tensile Strength Determination of Hot-Dip Plastic Coated Steel Pipes: Standards, Samples, and Test M

Hot-dip plastic coated steel pipes combine the load-bearing capacity of steel with the corrosion resistance of a bonded polymer layer, making tensile strength determination a critical step in quality control and product certification. This article explains how tensile strength testing of hot-dip plastic coated steel pipes is performed in accredited third-party laboratories in accordance with GB/T 228.1, ISO 6892-1, and ASTM A370, covering specimen preparation, tested parameters, calculation methods, and typical applications.

Technical Overview

Hot-dip plastic coated steel pipe is a composite product in which a seamless or welded steel pipe is heated and immersed in a fluidized bed of polymer powder, commonly epoxy, polyethylene (PE), or PVC-based materials, so that a continuous protective layer bonds to the internal and external surfaces. The steel substrate carries the mechanical and pressure loads, while the coating provides corrosion protection, chemical resistance, and a smooth, low-friction bore.

Because the coating process heats the pipe to temperatures typically between 180 °C and 300 °C, tensile strength determination is performed to confirm that this thermal cycle has not degraded the mechanical properties of the steel. Testing is normally carried out in accredited third-party laboratories or manufacturer laboratories using universal testing machines, in accordance with metallic tensile testing standards such as GB/T 228.1, ISO 6892-1, ASTM E8/E8M, and ASTM A370. Where the tensile properties of the coating material itself are required, plastics testing standards such as ISO 527-2, ASTM D638, and GB/T 1040.2 are applied.

Testing Samples

Longitudinal Strip Specimens

The most common specimen for pipe tensile testing is a rectangular strip cut parallel to the pipe axis, prepared in accordance with GB/T 228.1 or ASTM A370. The strip is straightened carefully without altering its cross-section, and the width and wall thickness are measured at several points along the gauge length to determine the original cross-sectional area. Proportional gauge lengths of 5.65 × √S0 or non-proportional gauge lengths of 50 mm may be used depending on the specification.

Full-Section Specimens

For small-diameter pipes from which flat strips cannot be obtained, full-section pipe specimens may be tested. Metal plugs are inserted into the ends of the specimen to prevent crushing in the grips, and the cross-sectional area of the pipe wall is used for stress calculation.

Transverse Weld Specimens

For welded hot-dip plastic coated pipes, transverse strip specimens containing the weld seam may be prepared to verify that the weld joint, which also passes through the heating cycle, retains adequate tensile strength.

Polymer Coating Specimens

When the tensile properties of the coating material are specified, dumbbell-shaped specimens, for example ISO 527-2 Type 1B or ASTM D638 Type I, are either cut from the coating where thickness permits or compression-molded from powder taken from the same production batch.

Testing Items

  • Tensile strength (Rm) of the steel substrate
  • Upper or lower yield strength (ReH, ReL) or 0.2% proof strength (Rp0.2)
  • Elongation after fracture (A or A50 mm)
  • Tensile strength of transverse weld specimens for welded pipes
  • Tensile strength, elongation at break, and elastic modulus of the polymer coating when specified

Acceptance criteria are defined by the applicable product standard. In general, the base steel of a coated composite pipe must still satisfy the mechanical requirements of the underlying steel pipe standard, such as GB/T 8163 for seamless pipes or GB/T 3091 for welded pipes, after the hot-dip coating process.

Testing Methods

Equipment and Calibration

A screw-driven or servo-hydraulic universal testing machine with force measurement accuracy of grade 1 or better per ISO 7500-1 or ASTM E4 is used. Extensometers used for determining yield strength should meet the accuracy classes of ISO 9513 or ASTM E83, and the machine must be verified at defined intervals with certified force proving devices.

Test Procedure

  • Condition the specimen, then measure and record the original cross-sectional area from the measured width and thickness or from pipe dimensional data.
  • Mark the original gauge length and apply reference marks for post-fracture elongation measurement.
  • Set the test speed in accordance with the specified method, using stress-rate or displacement-rate control per GB/T 228.1 or ASTM E8; strip specimens are commonly tested in the range of 2 to 30 mm/min.
  • Grip the specimen with wedge grips, ensuring axial alignment to minimize bending stresses.
  • Apply the load continuously until fracture and record the maximum force, the force-extension curve, and yield point data where required.
  • Reassemble the fractured pieces and measure the final gauge length to calculate elongation after fracture.
  • Conduct the test at room temperature between 10 °C and 35 °C unless otherwise specified.

Calculation of Results

Tensile strength is calculated as Rm = Fm / S0, where Fm is the maximum force and S0 is the original cross-sectional area, and is expressed in megapascals. Elongation after fracture is calculated as A = (Lu − L0) / L0 × 100%. For coating specimens, tensile strength is the maximum force divided by the initial cross-sectional area of the narrow section of the dumbbell. The results are compared against the minimum requirements of the applicable steel grade and product standard, and a test report is issued documenting specimen identification, dimensions, machine and extensometer data, test speed, results, and any observed anomalies.

Applications

  • Municipal and building water supply and distribution piping
  • Automatic fire sprinkler and standpipe systems
  • Underground cable protection conduits for power and telecommunications networks
  • Water, slurry, and ventilation piping in coal mines and tunnels
  • Chemical and industrial fluid transport requiring corrosion resistance
  • HVAC chilled water, condenser water, and district energy piping

FAQ

Why is tensile strength tested on the steel substrate of a coated pipe?

The steel substrate carries the structural and pressure loads, so its tensile properties determine whether the pipe can perform safely in service. Since the hot-dip process exposes the pipe to elevated temperatures, tensile testing verifies that this exposure has not reduced the strength or ductility of the base metal below the requirements of the original steel grade.

Does the plastic coating affect the measured tensile strength?

For substrate testing, the coating is normally removed from the specimens before testing so that the measured properties reflect the steel alone. The coating layer is thin relative to the pipe wall, but removing it avoids errors in cross-sectional area measurement and grip behavior.

What if the pipe diameter is too small for strip specimens?

Full-section tensile testing with plugged ends is used for small-diameter pipes, following the provisions of ASTM A370 and GB/T 228.1 for tubular products. The cross-sectional area of the pipe wall is used to compute the applied stress.

How many specimens should be tested?

Typical acceptance testing requires one or more specimens per heat, batch, or production lot as defined by the product standard or purchase specification. Accredited third-party laboratories usually recommend testing at least two or three specimens to account for material variability.

Can the tensile properties of the coating be tested as well?

Yes. When the specification requires coating mechanical data, dumbbell specimens are tested per ISO 527-2, ASTM D638, or GB/T 1040 to determine coating tensile strength, elongation at break, and modulus. Pull-off adhesion testing may complement these results to evaluate the coating-to-steel interface.

Why Choose ZKGX?

  • State-of-the-art analytical equipment
  • Highly qualified scientific team
  • Fast turnaround time
  • Competitive pricing