Swelling ratio testing to Chinese National Standards (GB standards) is a critical quality control method used to evaluate how rubber, elastomers, hydrogels, and superabsorbent materials absorb liquids and change in mass or volume under defined conditions. This article explains the governing GB test standards, typical sample types, measurement procedures, calculation formulas, and industrial applications of swelling ratio determination. Understanding these requirements helps manufacturers, suppliers, and accredited third-party laboratories ensure material compatibility and regulatory compliance.
Technical Overview
The swelling ratio (also called swelling degree or expansion ratio) is a quantitative measure of the mass or volume increase a material undergoes after exposure to a liquid medium such as oil, fuel, water, or a chemical reagent. It is a fundamental performance indicator for polymeric materials because excessive swelling signals poor liquid resistance, dimensional instability, and potential sealing failure, while negative values may indicate the extraction of plasticizers or soluble components.
In China, swelling ratio determination is governed by national standards (GB standards). The most widely applied standard is GB/T 1690, which specifies the determination of the resistance of vulcanized or thermoplastic rubbers to liquids and is technically aligned with ISO 1817. For hydrophilic water-swelling rubber products, GB 18173.3 defines the expansion ratio requirements and test method for waterproofing applications. Sample conditioning follows GB/T 2941, ensuring that temperature and humidity before measurement do not distort results.
The two principal expressions of the swelling ratio are:
- Mass swelling ratio: Qm = (m2 − m1) / m1 × 100%, where m1 is the initial mass and m2 is the mass after immersion.
- Volume swelling ratio: Qv = (V2 − V1) / V1 × 100%, where V1 is the initial volume and V2 is the volume after immersion.
Positive values indicate swelling; negative values indicate mass or volume loss, typically caused by the extraction of soluble ingredients or chemical degradation. Testing is routinely performed by accredited third-party laboratories to support product certification, incoming material inspection, and failure analysis.
Testing Samples
Vulcanized and Thermoplastic Rubber Compounds
Standard test pieces are typically cut from cured sheets, commonly 25 mm × 25 mm squares with a thickness of approximately 2 mm, as specified in GB/T 1690. Both vulcanized rubber compounds and thermoplastic elastomers can be evaluated, including NBR, EPDM, FKM, CR, and NR formulations.
Water-Swelling (Hydrophilic) Rubber Products
Finished products such as water-swelling seal strips, waterstops for construction joints, and hydrophilic rubber gaskets are tested to GB 18173.3. These products are designed to expand controllably in contact with water to create a compressive seal, so their maximum expansion ratio and expansion kinetics are decisive performance parameters.
Elastomeric Seals and O-Rings
Commercial-size seals, O-rings, gaskets, and diaphragms can be tested as finished articles when the end-use condition must be simulated. Testing actual components accounts for curing state, geometry, and surface effects that differ from flat laboratory sheets.
Superabsorbent Polymers and Hydrogels
SAP powders and granules used in hygiene products, as well as medical hydrogels for wound dressings and cold compress patches, are evaluated for free swelling capacity and retention performance using gravimetric absorption methods based on GB principles and equivalent international procedures.
Testing Items
Depending on the material and end-use requirement, a swelling ratio test program to GB standards may include the following measurable items:
- Mass change rate (mass swelling ratio) after immersion for a specified time and temperature.
- Volume change rate (volume swelling ratio) determined by the Archimedes displacement method.
- Dimensional change in length, width, and thickness after liquid exposure.
- Swelling kinetics — a time-dependent curve measured at multiple immersion intervals (for example, 2 h, 24 h, 48 h, 72 h, and 168 h).
- Extractable matter content, indicating loss of soluble components.
- Post-immersion changes in hardness, tensile strength, and elongation at break.
- Maximum expansion ratio for water-swelling rubber to GB 18173.3.
Testing Methods
The general gravimetric immersion procedure according to GB/T 1690 and related GB standards proceeds as follows:
- Conditioning: Specimens are conditioned at 23 ± 2 °C and 50 ± 5% relative humidity per GB/T 2941 until mass stabilization.
- Initial measurement: The initial mass m1 is measured on an analytical balance, and the initial volume V1 is determined by water displacement (Archimedes method), correcting for the suspension wire volume.
- Immersion: Specimens are fully immersed in the test liquid at the specified temperature. Common media include No. 1 and No. 3 standard reference oils, standard fuels, distilled water, salt solution, acids, alkalis, and service fluids. Typical test temperatures range from 23 °C up to 150 °C depending on the rubber class, and standard durations include 24 h, 70 h, and 168 h.
- Post-immersion handling: Specimens are removed, and surface liquid is quickly blotted within 30 seconds to avoid evaporation losses; the wet mass m2 and wet volume V2 are measured promptly.
- Calculation: The mass and volume swelling ratios are calculated using the formulas above, and results are reported as the median of at least three specimens.
- Supplementary testing: Hardness and tensile properties may be measured on specimens dried to constant mass to quantify permanent degradation.
For water-swelling rubber to GB 18173.3, specimens are immersed in distilled water at 23 °C and the expansion ratio is tracked at defined intervals to verify both the swelling rate and the maximum expansion ratio specified for the product grade. For superabsorbent polymers, free swell capacity is typically determined by allowing a weighed quantity of material to absorb excess liquid, followed by filtration or centrifugal removal of unabsorbed fluid and gravimetric determination of the absorbed amount.
Applications
Swelling ratio testing to GB standards supports material selection, qualification, and quality control across many industries:
- Automotive: Fuel hoses, oil seals, engine mounts, and brake components must resist swelling in fuels and lubricants over their service life.
- Construction and infrastructure: Water-swelling rubber waterstops and seal strips used in tunnels, basements, and precast joints rely on controlled expansion ratios for watertightness.
- Hygiene and consumer products: Superabsorbent polymers in diapers and incontinence products are qualified by their swelling and retention capacity.
- Medical devices: Hydrogel dressings, transdermal patches, and catheter materials are evaluated for absorption behavior and dimensional stability in body-simulating fluids.
- Pipelines and chemical processing: Gaskets, O-rings, and elastomeric liners exposed to process chemicals are validated against swelling limits to prevent leakage.
- Cable and electronics: Water-blocking tapes, potting gels, and sealing compounds are assessed for controlled water absorption.
FAQ
Which GB standard applies to my material?
For rubbers and thermoplastic elastomers immersed in oils, fuels, or chemicals, GB/T 1690 applies. For water-swelling rubber waterproofing products, GB 18173.3 applies. Sample preparation and conditioning requirements reference GB/T 2941. Accredited third-party laboratories can confirm the correct standard for a specific product.
What is the difference between mass swelling ratio and volume swelling ratio?
The mass swelling ratio is measured gravimetrically and reflects the net uptake of liquid, while the volume swelling ratio is measured by displacement and reflects dimensional change. The two values can differ when soluble components are simultaneously extracted from the material during immersion.
What test liquids and temperatures are used?
Common media include standard reference oils, standard fuels, distilled water, and service fluids, with test temperatures selected according to the rubber class and application, typically from room temperature up to 150 °C.
How long does a test take?
A single-point test at a standard duration such as 24 h or 70 h can be completed within a few working days including conditioning. Kinetic studies with multiple immersion intervals or equilibrium swelling determination may require one to two weeks.
What does a negative swelling ratio mean?
A negative value indicates the specimen lost mass or volume, usually due to the extraction of plasticizers, process oils, or other soluble additives, or due to chemical degradation of the polymer network.
Why Choose ZKGX?
- State-of-the-art analytical equipment
- Highly qualified scientific team
- Fast turnaround time
- Competitive pricing