Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Spherical Bearing Aging Performance Testing: Standards, Methods, and Evaluation

Spherical bearing aging performance testing evaluates the long-term durability of bridge and structural bearings by subjecting their elastomeric, PTFE, and metallic components to accelerated thermal, oxidative, and mechanical aging conditions. This testing is essential for verifying that spherical bearings can maintain their load-bearing capacity, friction coefficient, and rotational function throughout a design service life that often exceeds 50 to 100 years. Accredited third-party laboratories perform these tests in accordance with international and national standards such as GB/T 17955, EN 1337, and ISO 1431.

Technical Overview

Spherical bearings (also known as spherical pot-type or spherical structural bearings) are mechanical devices installed between a bridge superstructure and its substructure to accommodate rotation, translation, and vertical load transfer. A typical spherical bearing consists of a convex spherical steel segment, a concave counter-surface, a low-friction sliding material such as polytetrafluoroethylene (PTFE) or ultra-high-molecular-weight polyethylene (UHMWPE), an elastomeric sealing system, and anchored steel housings. Because these bearings are expected to function for decades without replacement, aging performance testing is a critical part of product qualification and type testing.

Aging performance testing simulates the cumulative degradation that occurs in service due to heat, oxygen, ozone, ultraviolet exposure, moisture, and sustained mechanical stress. The polymeric components—particularly the sliding interface material and elastomeric seals—are most susceptible to deterioration, which can manifest as increased friction coefficient, dimensional change, hardening, cracking, loss of sealing integrity, or reduced mechanical strength. Accelerated aging protocols expose specimens to elevated temperatures and controlled atmospheres for defined durations, after which retained properties are compared against minimum acceptance criteria specified in the applicable product standards.

The governing reference standards for this field include GB/T 17955 for bridge spherical bearings, EN 1337 series for structural bearings in Europe, GB/T 20688 series for elastomeric seismic isolators and bearings, ISO 188 for accelerated aging of vulcanized rubber, ISO 1431 for ozone resistance, and ASTM D573 for rubber deterioration in an air oven. Together, these standards define specimen preparation, aging conditions, post-aging test methods, and acceptance thresholds.

Testing Samples

PTFE and UHMWPE Sliding Plates

Sliding plate specimens are cut from production-grade PTFE or UHMWPE sheets, typically with the same dimple pattern and silicone grease lubrication used in the finished bearing. These coupons are aged to evaluate changes in friction coefficient, wear rate, compressive creep, and dimensional stability.

Elastomeric Components and Seals

Rubber seals, sealing rings, and any elastomeric damping elements are sampled as standard tensile dumbbell specimens and compression-set buttons. The compound is usually natural rubber, chloroprene rubber (CR), or ethylene propylene diene monomer (EPDM), and aging tests measure the retention of hardness, tensile strength, elongation at break, and compression set.

Complete Bearing Assemblies

Full-scale spherical bearings are tested to assess system-level aging behavior, including the interaction between the sliding surfaces, seals, and steel components after prolonged loading and thermal conditioning. Assembly tests verify rotational performance, vertical stiffness, and friction behavior following accelerated exposure.

Metallic Components and Coatings

Steel segments, anchor plates, and protective coatings (such as zinc-rich primers or thermal-sprayed metal coatings) are evaluated for corrosion aging resistance through neutral salt spray exposure and cyclic corrosion testing in accordance with ISO 9227 and ASTM B117.

Testing Items

A comprehensive aging performance evaluation of spherical bearings typically includes the following test items:

  • Hot air accelerated aging of elastomeric compounds at 70°C, 85°C, or 100°C for 70 to 168 hours, followed by measurement of hardness change, tensile strength retention, and elongation retention.
  • Friction coefficient determination on sliding plates before and after thermal aging, verified under design vertical stress with a defined sliding path.
  • Compressive creep and permanent deformation testing of PTFE/UHMWPE plates under sustained design load.
  • Compression set testing of elastomeric seals after aging.
  • Ozone resistance testing of rubber seals under static and dynamic strain conditions per ISO 1431-1.
  • Low-temperature flexibility and brittleness testing to confirm performance after cold-region exposure.
  • Line wear and cumulative wear measurement of the sliding interface after repeated cyclic displacement.
  • Rotational performance verification of complete assemblies after aging conditioning.
  • Adhesion and cohesion assessment of bonding layers between polymer and substrate.
  • Salt spray corrosion resistance of steel components and protective coating systems.

Testing Methods

Aging tests are conducted using forced-ventilation hot air ovens with temperature uniformity of ±1°C to ensure reproducible degradation kinetics. Elastomeric specimens are conditioned at selected temperatures, then cooled to standard laboratory temperature before post-aging properties are measured. Property retention is calculated as the percentage ratio of aged to unaged values, and results must satisfy the minimum thresholds defined by the referenced standard—for example, tensile strength and elongation retention commonly exceeding 80 to 90 percent depending on the compound class and product specification.

Friction and wear testing is performed on dedicated bearing test rigs that apply the design vertical compressive stress (commonly 24 to 30 MPa for PTFE) while cycling the sliding plate through a prescribed stroke path. The apparent friction coefficient is recorded as the ratio of horizontal to vertical force and compared against the specified upper limit both in the as-received condition and after aging. Long-stroke and short-stroke cycling may be combined to accumulate the total travel distance required by the standard.

Ozone resistance is evaluated by exposing strained rubber specimens to an ozone-containing atmosphere at controlled concentration (such as 50 pphm), temperature, and duration, then examining the surface for cracks under magnification. Corrosion aging of metallic parts uses neutral salt spray chambers or cyclic wet-dry corrosion cabinets, with coating integrity, blistering, and red rust formation rated after exposure. Complete assemblies may undergo combined conditioning—sustained compression plus thermal cycling—followed by functional rotation and friction verification to demonstrate that aged bearings continue to meet design performance requirements.

Applications

Aging performance testing of spherical bearings supports a wide range of engineering and regulatory applications:

  • Product type testing and first-article qualification for new spherical bearing designs prior to installation on highway, rail, and high-speed railway bridges.
  • Factory production control and periodic batch verification by bearing manufacturers to demonstrate continued conformity.
  • Independent conformity assessment by accredited third-party laboratories for tender submissions, CE marking under the EN 1337 framework, and certification against GB/T 17955 requirements.
  • Condition assessment and remaining service life estimation of in-service bearings during bridge inspection, maintenance planning, and retrofit programs.
  • Research and development of new sliding materials, lubricant systems, and sealing compounds with improved long-term durability.
  • Acceptance testing for bearings installed in high-temperature, cold-region, coastal, or high-pollution environments where aging mechanisms are accelerated.

FAQ

What is the typical design service life assumed in aging tests?

Standards for structural spherical bearings generally assume a service life of 50 to 100 years. Because real-time verification is impractical, accelerated aging at elevated temperatures with time-temperature extrapolation (based on Arrhenius-type kinetics) is used to estimate long-term property retention and to set acceptance criteria for short-duration laboratory aging.

Which components of a spherical bearing are most affected by aging?

The polymeric elements—the PTFE or UHMWPE sliding plate, silicone grease lubricant, and elastomeric seals—degrade most significantly. Typical aging effects include rising friction coefficient, creep deformation of the sliding plate, hardening and ozone cracking of rubber seals, and slow depletion of lubricant. Steel components degrade mainly through corrosion, which is addressed with protective coatings and salt spray testing.

What acceptance criteria are commonly applied after aging?

Common criteria include tensile strength and elongation retention of at least 80 to 90 percent, hardness change within a defined band (often ±6 to ±10 IRHD), compression set below a specified maximum, no visible ozone cracking at stated magnification, and a friction coefficient of the aged sliding interface that remains below the design limit, typically on the order of 0.03 to 0.05 for lubricated PTFE at design stress.

How long does a complete aging test program take?

Simple hot air aging plus post-aging mechanical testing can be completed within one to two weeks. Programs that include full-scale assembly conditioning, long-distance sliding wear accumulation, cyclic corrosion exposure, and ozone testing may extend from several weeks to several months depending on the specified durations and the number of test items.

Can aged in-service bearings be evaluated?

Yes. Witness coupons or extracted samples from in-service bearings can be tested for retained mechanical properties, friction coefficient, and wear depth. The results are compared with the original specification to judge whether the bearing remains fit for continued service or should be scheduled for replacement.

Why Choose ZKGX?

  • State-of-the-art analytical equipment
  • Highly qualified scientific team
  • Fast turnaround time
  • Competitive pricing