Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Microhardness Testing of Nitrided Layers: Methods, Standards, and Applications

Nitrided layer microhardness testing is the primary quality-control method for verifying the surface hardness, hardness gradient, and effective case depth of nitrided steel components. Using low-force Vickers or Knoop indentation in accordance with ASTM E384, ISO 6507, and GB/T 11354, the test confirms that thermochemical surface hardening has achieved the hardness and depth required by the product specification. This article explains the test principle, sample preparation, measurement procedures, acceptance criteria, and typical industrial applications.

Technical Overview

Nitriding is a thermochemical surface hardening process in which nitrogen diffuses into the surface of a steel component at temperatures of approximately 500 °C to 580 °C, using gas, plasma, or salt-bath media. The treatment produces a hard, wear-resistant, corrosion-resistant case without subsequent quenching, and with minimal distortion of the part. A typical nitrided case consists of a thin compound layer (often called the white layer) composed of iron nitrides, usually 5 µm to 30 µm thick, over a deeper diffusion zone in which very fine alloy nitrides precipitate and raise the hardness of the matrix.

Depending on the alloy content of the steel, the case hardness may range from roughly 300 HV on unalloyed carbon steels to 1200 HV or higher on dedicated nitriding steels and hot-work tool steels. Because the hardened case is thin—commonly 0.1 mm to 0.8 mm total—and because the hardness falls steeply beneath the surface, conventional macro-hardness tests such as Rockwell or Brinell are unsuitable: the larger indentations penetrate through the case and return a composite value influenced by the softer core. Microhardness testing with low indentation forces, typically 10 gf to 1000 gf (HV0.01 to HV1), confines the plastic zone within the case and allows the hardness to be measured as a function of depth.

Nitrided layer microhardness testing is performed by in-house metallurgical laboratories and by accredited third-party laboratories, and it serves as the objective basis for acceptance of nitrided parts, process qualification, and failure analysis. The governing methods and application standards include ASTM E384 and ASTM E92, ISO 6507, GB/T 4340.1, and GB/T 11354 for nitrided layer depth and microstructure evaluation.

Testing Samples

Cross-Sectional Metallographic Samples

The standard sample is a full cross-section cut perpendicular to the nitrided surface. Cutting must be performed with abundant coolant to avoid overheating, which would locally temper or alter the case. The specimen is mounted in epoxy or bakelite using practices that preserve the edge—such as face-to-face clamping of two nitrided surfaces, or backing with electroplated nickel—because a rounded edge causes artificially low readings near the surface. The mount is ground through successive abrasive grades and polished to a 1 µm diamond or finer finish. Etching with 2% to 4% nital is applied after the hardness measurements when microstructural evaluation is also required.

Whole Small Components and Witness Coupons

Small parts such as valve stems, pins, nozzles, and screws can often be mounted and sectioned whole. For large or expensive components, witness coupons of the same steel grade are nitrided together with the production load and sectioned for evaluation, provided coupon geometry and surface condition represent the actual parts.

Prepared Flat Surfaces for Surface Hardness Testing

When only surface hardness is required and the part geometry permits, a small flat area of the actual component can be locally ground and polished in situ. This semi-destructive approach supports routine statistical process control without sacrificing the entire part.

Testing Items

A complete microhardness evaluation of a nitrided part typically includes the following measurable items:

  • Case surface microhardness, reported with the test force, for example 950 HV0.5 or 1050 HV0.1
  • Compound (white) layer microhardness at very low loads such as HV0.025 to HV0.05
  • Microhardness gradient, a hardness-versus-depth profile from the surface into the unaffected core
  • Nitriding hardness depth (NHD, also known as Nht or effective case depth), the distance from the surface to the specified hardness limit
  • Circumferential and positional hardness uniformity around the part and across the batch
  • Compound layer brittleness rating based on the cracking behavior of a heavier Vickers indentation on the nitrided surface

Each item addresses a distinct failure mode: surface hardness governs wear resistance, the gradient governs load-bearing capacity, case depth governs fatigue and spalling resistance, and brittleness rating flags an overly brittle compound layer that could crack or exfoliate in service.

Testing Methods

Vickers Microhardness Testing

The Vickers method uses a diamond pyramid with a 136° included angle, and it is the primary technique for nitrided layers. Procedures follow ASTM E384, ASTM E92, ISO 6507-1, and GB/T 4340.1. The full-length diagonals of the indentation are measured optically, and the HV value is calculated from the applied force and the surface area of the indentation. Because the case hardness changes steeply with depth, the indentation must be kept small; a practical rule from ASTM E384 is that the distance from the center of an indentation to the specimen edge, or to a neighboring indentation, should be at least 2.5 times the diagonal length.

Knoop Microhardness Testing

For very thin compound layers or steep gradients, the Knoop indenter is advantageous. Its elongated rhombic geometry, with an approximately 7:1 diagonal ratio and shallower penetration, allows the long diagonal to be oriented parallel to the surface so that measurements can be made closer to the outer edge with less disturbance from the underlying diffusion zone. Knoop testing is also covered by ASTM E92 and ASTM E384.

Hardness Traverse and Case Depth Determination

The nitriding hardness depth is determined by a series of indentations made at known distances from the nitrided surface, either along a line running inward from the edge or in staggered rows at increasing depth. Typical indentation spacing is 0.05 mm to 0.10 mm near the surface, widening in the transition zone. Hardness is plotted against depth, and the effective case depth is taken at the depth where the hardness falls to the specified limit—most commonly 50 HV above the measured core hardness, consistent with international case-depth conventions such as ISO 18203, unless the product drawing specifies an absolute limit such as 550 HV. The boundary depth is obtained by interpolation between the two indentations that straddle the limit value, and the result is reported to the nearest 0.01 mm or 0.05 mm as required.

Test Force Selection

The test force is selected as a compromise between measurement precision and spatial resolution. Forces of HV0.01 to HV0.05 are used inside the compound layer, HV0.1 to HV0.5 for near-surface case hardness, and HV0.5 to HV1 for traverses where the case is sufficiently thick. Every reported result must include the force designation, because the measured hardness of a gradient structure increases as the force decreases and the indentation samples less of the softer underlying material.

Brittleness Evaluation of the Compound Layer

For components subject to contact loading, a heavier Vickers indentation (commonly HV5 or HV10, depending on the specification) is placed on the nitrided surface and the indentation corners are examined for cracks. The severity of cracking is graded on a scale from 1 (sound) to 5 (severely cracked), with acceptance limits defined by the applicable product standard or customer drawing, following the practice described in GB/T 11354.

Applications

Nitrided layer microhardness testing is applied wherever nitriding, nitrocarburizing, or plasma nitriding is used to enhance wear resistance, fatigue strength, scuffing resistance, or corrosion resistance. Typical applications include:

  • Automotive powertrain components such as crankshafts, camshafts, tappets, valve stems, and transmission gears
  • Plastic injection and die-casting tooling, extruder screws, and barrel liners made from hot-work tool steels such as H13
  • Hydraulic and fluid-power components including pump plungers, cylinder rods, spools, and valve gates
  • Aerospace and energy-industry parts such as actuator components, bearing journals, and gas-turbine hardware
  • Textile, food-processing, and general machinery parts where galling, fretting, or adhesive wear must be controlled
  • Process qualification, incoming inspection, supplier verification, and root-cause failure analysis of premature wear or case spalling

In all of these contexts, the microhardness profile provides the quantitative link between the heat-treatment process parameters and the functional performance of the component.

FAQ

Why is microhardness used instead of Rockwell testing for nitrided layers?

Nitrided cases are typically thinner than 1 mm and much harder than the core. Rockwell and Brinell indentations are too large and deep, so they measure a composite of case and core and cannot resolve the hardness gradient. Low-force Vickers or Knoop indentations remain within the case and can be positioned at specific depths to map the profile.

What test force should be selected?

Choose the largest force that still keeps the indentation within the region of interest while respecting the minimum edge and spacing distances of 2.5 times the diagonal. In practice, HV0.01 to HV0.05 suits the compound layer, HV0.1 to HV0.5 suits near-surface case hardness, and up to HV1 may be used for thick cases. Always report the force together with the hardness value.

How is the effective nitriding depth defined?

The effective depth is the distance from the surface to the point where the hardness falls to a specified limit. Unless the drawing states an absolute value, the limit is usually taken as 50 HV above the core hardness. The depth is found by interpolation from a hardness-depth traverse and is reported in millimeters.

What hardness values are typical for nitrided steels?

Unalloyed steels typically reach 300 HV to 450 HV in the diffusion zone, chromium-molybdenum alloy steels such as 42CrMo4 reach approximately 550 HV to 750 HV, dedicated nitriding steels such as 41CrAlMo7 reach 900 HV to 1200 HV, and nitrided hot-work tool steels can exceed 1000 HV to 1300 HV. Acceptance values must always be agreed against the specific steel grade and application.

Should the sample be etched before or after indentation?

Indentations should be made on the final polished, unetched surface, because etching can produce surface relief and staining that degrade diagonal measurement. Etching with nital is performed afterwards if the microstructure, compound layer morphology, or porosity must also be evaluated.

Can testing be performed on real parts without destroying them?

Surface hardness can be checked semi-destructively on an accessible, locally polished area of the actual component. Determination of case depth, however, requires a full cross-section, so witness coupons nitrided with the production load are commonly used to represent large or high-value parts.

Why Choose ZKGX?

  • State-of-the-art analytical equipment
  • Highly qualified scientific team
  • Fast turnaround time
  • Competitive pricing