Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

ASTM G67 Intergranular Corrosion Testing of 5XXX Series Aluminum Alloys (NAMLT Test)

ASTM G67, also known as the Nitric Acid Mass Loss Test (NAMLT), is the internationally recognized standard test method for determining the susceptibility of 5XXX series aluminum alloys to intergranular corrosion. By measuring mass loss after exposure to concentrated nitric acid at 30 °C for 24 hours, the test quantifies the degree of sensitization caused by anodic beta-phase precipitation at grain boundaries. This article explains the testing principle, sample requirements, procedure, evaluation criteria, and typical industrial applications of ASTM G67.

Technical Overview

ASTM G67 is the Standard Test Method for Determining the Susceptibility to Intergranular Corrosion of 5XXX Series Aluminum Alloys by Mass Loss After Exposure to Nitric Acid, commonly abbreviated as the NAMLT test. It applies to aluminum-magnesium (Al-Mg) alloys such as 5083, 5086, 5456, 5454, and 5059, which are widely used in marine, cryogenic, and structural applications.

The underlying mechanism of the test relates to sensitization. When 5XXX series alloys are exposed to elevated temperatures (typically in the range of approximately 50 °C to 200 °C) for extended periods, the beta phase (β-Al3Mg2) precipitates preferentially along grain boundaries. This beta phase is electrochemically anodic relative to the aluminum matrix. In concentrated nitric acid, the beta phase dissolves rapidly and selectively, producing intergranular attack and, in severely sensitized material, grain dropping.

Because the mass loss per unit area correlates directly with the amount of grain-boundary beta phase present, the NAMLT result is widely used as a quantitative measure of the degree of sensitization (DoS). Elevated NAMLT values also correlate with increased susceptibility to exfoliation corrosion and stress corrosion cracking, which are evaluated separately by standards such as ASTM G66 and ASTM G44. It should be noted that ASTM G67 is specific to the 5XXX series; exfoliation testing of 2XXX and 7XXX alloys is covered by ASTM G34.

Testing Samples

Applicable Materials and Product Forms

ASTM G67 applies to wrought products of 5XXX series aluminum-magnesium alloys, including plate, sheet, extrusions, forgings, and pipe. Typical grades tested include 5052, 5083, 5086, 5454, 5456, 5754, and 5059 in tempers such as H116, H321, H131, and O/H111 conditions. Welded assemblies can also be evaluated, particularly to assess the sensitization behavior of the heat-affected zone (HAZ) and base metal after fabrication or service exposure.

Specimen Preparation Requirements

  • Specimen dimensions are nominally 50 mm by 25 mm, with the product thickness retained up to a maximum of 25 mm; thicker products are machined down from one face to represent the mid-thickness microstructure.
  • All surfaces are machined or prepared to remove scale, coarse tool marks, and any pre-existing corrosion damage that could distort the mass loss result.
  • Prior to testing, specimens are degreased, chemically cleaned by alkaline etching and nitric acid desmutting in accordance with the standard, thoroughly rinsed, dried, and weighed on an analytical balance.
  • The exact exposed surface area of each specimen is calculated from its measured dimensions, as all faces and edges are exposed to the acid.
  • Testing of multiple specimens (typically three per material condition) is recommended to improve the reliability of the reported result.

Testing Items

The primary measured quantity in ASTM G67 is the nitric acid mass loss, expressed in milligrams per square centimeter (mg/cm²), which represents the degree of sensitization of the material. Supporting evaluations may include visual examination for exfoliation or grain dropping, and metallographic cross-sectioning to confirm the intergranular nature of the attack.

Evaluation Criteria

  • Mass loss below approximately 15 mg/cm² generally indicates low susceptibility to intergranular corrosion.
  • Mass loss between approximately 15 and 25 mg/cm² indicates moderate or intermediate susceptibility.
  • Mass loss above approximately 25 mg/cm² indicates high susceptibility, and very high values (roughly above 35 to 40 mg/cm²) are associated with severe sensitization, grain dropping, and a high risk of exfoliation and stress corrosion cracking.
  • Formal acceptance limits are defined by the governing product specifications rather than by ASTM G67 itself; for example, marine-grade tempers such as H116 and H321 are qualified with NAMLT requirements referenced in specifications such as ASTM B928.

Testing Methods

Test Procedure

The ASTM G67 test is performed by accredited third-party laboratories and in-house materials laboratories using the following sequence:

  • Clean, dry, and weigh each prepared specimen to the required precision on an analytical balance.
  • Immerse the specimens fully in concentrated nitric acid (minimum 70 % HNO3) maintained at 30 °C ± 1 °C for a continuous exposure period of 24 hours, ensuring the minimum acid volume-to-surface-area ratio specified by the standard is met.
  • After exposure, remove the specimens, rinse them thoroughly, remove any adherent corrosion products in accordance with the standard, dry, and reweigh.
  • Calculate the mass loss per unit area as the difference between the initial and final masses divided by the exposed surface area, reported in mg/cm².
  • Report the NAMLT value for each specimen, the average value, the material identification, product form, temper, and any relevant metallurgical condition such as sensitization heat treatment or service history.

Equipment, Reagents, and Quality Control

The test requires a temperature-controlled water or oil bath, acid-resistant immersion vessels, concentrated nitric acid of specified purity, calibrated thermometers, and an analytical balance. Critical quality control points include strict temperature regulation at 30 °C ± 1 °C, use of fresh acid for each test run to prevent depletion effects, avoidance of excessive specimen loading in the acid, and replicate testing for statistical confidence. Because concentrated nitric acid is highly corrosive and evolves toxic fumes, all operations must be conducted under a fume hood with appropriate personal protective equipment and laboratory safety protocols.

Factors Affecting Results

Key variables that influence NAMLT results include the degree of sensitization of the material, specimen surface preparation, acid concentration and temperature stability, exposure duration, and the ratio of acid volume to specimen area. Careful control of these parameters is essential for reproducible results, and interlaboratory agreement is generally best in the low-to-moderate susceptibility range.

Applications

ASTM G67 testing supports quality assurance, materials qualification, failure analysis, and research across multiple industries:

  • Marine and shipbuilding: qualification of hull plates and structural members in 5083, 5086, and 5456 alloys for H116/H321 marine tempers, and assessment of in-service sensitization of vessels operating in warm seawater environments.
  • Cryogenic and LNG applications: verification that Al-Mg alloy plates and piping for liquefied natural gas containment systems remain unsensitized after fabrication and service.
  • Defense and armored vehicles: evaluation of sensitization in armor-grade 5XXX alloys subjected to ballistic heating, engine compartment temperatures, or desert service conditions.
  • Offshore, bridge, and rail structures: condition assessment of welded structures after prolonged thermal exposure or fire damage.
  • Research and development: quantification of degree of sensitization in studies of thermomechanical processing, stabilization treatments, retrogression and re-ageing, and new alloy development.
  • Weld procedure qualification: characterization of base metal and heat-affected zone corrosion behavior following welding thermal cycles.

FAQ

What does NAMLT stand for?

NAMLT stands for Nitric Acid Mass Loss Test. It is the common name for the ASTM G67 test method, in which the susceptibility to intergranular corrosion of 5XXX series aluminum alloys is quantified by the mass loss measured after 24 hours of immersion in concentrated nitric acid at 30 °C.

What NAMLT value is considered acceptable?

As a general guideline, values below approximately 15 mg/cm² indicate low susceptibility, 15 to 25 mg/cm² moderate susceptibility, and values above 25 mg/cm² high susceptibility. The definitive acceptance limit, however, is set by the applicable product specification or end-user requirement; marine-tempers such as H116 and H321 are typically qualified against NAMLT limits referenced in specifications like ASTM B928.

How does ASTM G67 differ from ASTM G66?

ASTM G67 (NAMLT) is a quantitative mass-loss method for 5XXX alloys that directly measures the degree of sensitization in mg/cm². ASTM G66 (EXCO test) is a complementary exfoliation corrosion test for the same alloy series that rates attack visually after exposure to an acidic chloride solution. The two methods are often performed together to provide a complete corrosion susceptibility profile.

Why is nitric acid used in the test?

Concentrated nitric acid selectively dissolves the anodic beta phase (Al3Mg2) that precipitates at grain boundaries during sensitization. The resulting mass loss is therefore directly proportional to the amount of grain-boundary beta phase, providing a reliable, quantitative indicator of intergranular corrosion susceptibility.

Can welded or in-service components be tested?

Yes. Specimens can be removed from welded fabrications, heat-affected zones, or components that have experienced service exposure. Testing in-service material is a common practice for condition monitoring, remaining-life assessment, and post-fire or post-incident investigations.

How long does an ASTM G67 test take?

The acid exposure itself lasts 24 hours. Including specimen machining, cleaning, weighing, and reporting, accredited third-party laboratories typically complete a standard test program within approximately three to seven working days, depending on the number of material conditions evaluated.

Why Choose ZKGX?

  • State-of-the-art analytical equipment
  • Highly qualified scientific team
  • Fast turnaround time
  • Competitive pricing